Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.560 J/g-°C @Temperature 500 °C |
0.134 BTU/lb-°F @Temperature 932 °F |
|
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |