Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.536 J/g-°C @Temperature 600 °C |
0.128 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® alloy, flat products Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.536 J/g-°C @Temperature 600 °C |
0.128 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.536 J/g-°C @Temperature 600 °C |
0.128 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.536 J/g-°C @Temperature 600 °C |
0.128 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.536 J/g-°C @Temperature 600 °C |
0.128 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.536 J/g-°C @Temperature 600 °C |
0.128 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.536 J/g-°C @Temperature 600 °C |
0.128 BTU/lb-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Specific Heat Capacity | 0.536 J/g-°C @Temperature 299 °C |
0.128 BTU/lb-°F @Temperature 570 °F |
|
Bohler-Uddeholm BeCu Alloy 172 Mold Material Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha.. |