Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, SMAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GTAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |