Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 20.0 - 100 °C |
0.108 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel Characteristics:Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Go.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |