Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.439 J/g-°C @Temperature 300 °C |
0.105 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 300 °C |
0.105 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 300 °C |
0.105 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 300 °C |
0.105 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 300 °C |
0.105 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 0.000 °C |
0.105 BTU/lb-°F @Temperature 32.0 °F |
|
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy) Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 300 °C |
0.105 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 300 °C |
0.105 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |