Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.381 J/g-°C @Temperature 20.0 °C |
0.0910 BTU/lb-°F @Temperature 68.0 °F |
|
Bohler-Uddeholm BeCu Alloy 172 Mold Material Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha.. |