Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Vaporization | 69.0 J/g | 29.7 BTU/lb | Latent, at normal boiling point |
3M Fluorinert™ FC-40 Electronic Liquid 3M™ Fluorinert™ Liquid FC-40 is a non-conductive, thermally and chemically stable fluid ideal for single phase heat transfer fluid applications, especially in the electronics and semiconductor ind.. |
|||
Heat of Vaporization | 69.0 J/g | 29.7 BTU/lb | Latent, at normal boiling point |
3M Fluorinert™ FC-70 Electronic Liquid Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a.. |