Polymer Property : Heat of Vaporization = 489 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Vaporization 489 J/g
210 BTU/lb
@ B.P.
LG Chemical Phenol
Structure & Characteristics: C6H5OH. Phenol is a white crystalline solid with a distinct smellUses: Raw material of phenolic resins, dye stuffs, synthetic fibers, herbicides, photo material, aromati..