Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 135 °C | 275 °F | ASTM D648 |
Kotec Carbotex K-75E Polycarbonate, Extrusion Grade Features: Extrusion, High viscosity, Natural transparentApplications: Sheets FilmsInformation provided by Kotec Corporation |
|||
Heat Distortion Temperature | 135 °C | 275 °F | ASTM D648 |
Kotec Carbotex K-75EUV Polycarbonate, Extrusion, UV Stability Grade Features: Extrusion, High viscosity, UV stability, Blue tintsApplications: Sheets FilmsInformation provided by Kotec Corporation |
|||
Heat Distortion Temperature | 135 °C | 275 °F | ASTM D648 |
Kotec Carbotex KV-75FD Polycarbonate, Food Grade Features: Food contact, High viscosity, Mold release, TransparentApplications: Household appliance, Kitchenware, Food packaging/containersInformation provided by Kotec Corporation |
|||
Heat Distortion Temperature | 135 °C | 275 °F | ISO 75-2 |
Tisan TISARBON® Flame Retardant (V0) Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Heat Distortion Temperature | 135 °C | 275 °F | ISO 75-2 |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Heat Distortion Temperature | 135 °C | 275 °F | ISO 75-2 |
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |