Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 200 °C | 392 °F | ISO 75 A/B |
Tisan TISAPET® UNR Polyethylene Terephthalate Properties:Excellent mechanical propertiesHigh thermal-chemical friction resistanceGood electrical propertiesGood rate of melt flow index relative to the quantity of glass fiberBalanced electrical a.. |
|||
Heat Distortion Temperature | 200 °C | 392 °F | ISO 75-2 |
Tisan TISLAMID® 6 30% Glass Bead Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Heat Distortion Temperature | 200 °C | 392 °F | ISO 75-2 |
Tisan TISLAMID® 6 30% Mineral Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |