Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Heat Distortion Temperature = 146 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat Distortion Temperature 146 °C
295 °F
ASTM D648
Kotec Carbotex KG-30MRA Polycarbonate, 30% Glass Fiber Reinforced
Features: Glass fiber 30% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E ..
Heat Distortion Temperature 146 °C
295 °F
ASTM D648
Kotec Carbotex KGN-30MRA Polycarbonate, Flame Retardant, 30% Glass Fiber Reinforced
Features: Glass fiber 30% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E ..
Copyright © lookpolymers.com All Rights Reserved