Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG34LG ABS Automotive: Low gloss ABS for unpainted interior applications. |
|||
CTE, linear, Transverse to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® MG34LG ABS Automotive: Low gloss ABS for unpainted interior applications. |
|||
CTE, linear, Transverse to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG34LGHF ABS Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® MG34LGHF ABS Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 93.6 µm/m-°C @Temperature 25.6 - 149 °C |
52.0 µin/in-°F @Temperature 78.0 - 300 °F |
Diameter |
Saint-Gobain Rulon® 488 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
CTE, linear, Transverse to Flow | 93.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Flame Retardant.. |
|||
CTE, linear, Transverse to Flow | 93.6 µm/m-°C @Temperature 25.6 - 149 °C |
52.0 µin/in-°F @Temperature 78.0 - 300 °F |
Diameter |
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f.. |