Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
46.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature 100 - 200 °C |
46.1 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve .. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature 100 - 200 °C |
46.1 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
46.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
46.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Asia Pacific) PPE+PS, HDT 125 |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
46.1 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
46.1 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
(Unverified Data**) Zytel® FG77G33L NC010 is a 33% glass fiber reinforced polyamide 612 resin for injection molding. It has been developed for consideration for applications such as parts in the food industry.Informat.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
46.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
CTE, linear, Transverse to Flow | 83.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
46.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |