Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Europe-Africa-Middle East) High flow PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Asia Pacific) Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 4401R PPC+PC LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Asia Pacific) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXM4701 PPC LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Americas .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXRL0683 PC Copolymer 11 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer 7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X2420 PC+POLYESTER (Asia Pacific) Xenoy*X2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad co.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Asia Pacific) Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7010HF PPE+PS Noryl* NH7010HF resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight par.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FP3060 PPE+PS (Europe-Africa-Middle East) Noryl* FP3060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |