Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 73.4 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 Eco-FR compound |
|||
CTE, linear, Transverse to Flow | 73.4 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP KONDUIT PX11311U PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 compliant with ECO protocols, non-brominated, non chlorinated |
|||
CTE, linear, Transverse to Flow | 73.5 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DEI13F PC LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R.. |