Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer (Asia Pacific) Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 160 - 249 °C |
36.1 µin/in-°F @Temperature 320 - 480 °F |
ASTM E228 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 100 - 200 °C |
36.1 µin/in-°F @Temperature 212 - 392 °F |
ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-7-190BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 100 - 200 °C |
36.1 µin/in-°F @Temperature 212 - 392 °F |
ISO 11359-2 |
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
CTE, linear, Transverse to Flow | 64.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
36.1 µin/in-°F @Temperature -58.0 - 122 °F |
ISO 11359-2 |
Chevron Phillips Xtel® XE5030BL Polyphenylene Sulfide Alloy Xtel® XE5030BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevr.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 55.0 - 160 °C |
36.1 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |