Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 50.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
CTE, linear, Transverse to Flow | 50.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific) LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
CTE, linear, Transverse to Flow | 50.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP UF0067W PPA LNP* THERMOCOMP* UF0067W is a compound based on Polyphthalamide resin containing 30% glass fiber. Added features of this material include: Hot Water Moldable, Non-Brominated & Non-Chlorinated Flam.. |
|||
CTE, linear, Transverse to Flow | 50.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DDF029 PC LNP STAT-KON* DDF029 is a compound based on Polycarbonate resin containing Carbon, Glass Fiber. Added features of this material include: Electrically Conductive. Flame Retardant. |