Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK LNP* LUBRICOMP* LCL33 is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold .. |
|||
CTE, linear, Transverse to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific) LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret.. |
|||
CTE, linear, Transverse to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
CTE, linear, Transverse to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC (Asia Pacific) LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
CTE, linear, Transverse to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Verton WV00A PBT (Europe-Africa-Middle East) LNP VERTON* WV00A is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Verton WV00A PBT (Europe-Africa-Middle East) LNP VERTON* WV00A is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |