Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon EE005 PEI
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-kon EE005 PEI
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-kon EE005 PEI (Asia Pacific)
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon EE005 PEI (Asia Pacific)
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON EE005E PEI
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON EE005E PEI
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON EE005E PEI (Asia Pacific)
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON EE005E PEI (Asia Pacific)
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI (Asia Pacific)
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 27.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
15.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI (Asia Pacific)
LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.