Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature 55.0 - 160 °C |
54.4 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature 55.0 - 160 °C |
54.4 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature 100 - 200 °C |
54.4 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4-230NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compare.. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature 100 - 200 °C |
54.4 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-230BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compared to oth.. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature 100 - 200 °C |
54.4 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surf.. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature 100 - 200 °C |
54.4 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Chevron Phillips Ryton® BR42C Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® BR42C is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surface fric.. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing 15% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing 10% PTFE, 15% Aramid. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 364 PBT+PC Designed for outdoor telecommunications enclosure applications. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 150 °C |
54.4 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 150 °C |
54.4 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
54.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8303 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized. For In Mold Decoration /Labeling. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
54.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
54.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
54.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 150 °C |
54.4 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
CTE, linear, Transverse to Flow | 98.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
54.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific) Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized |