Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 51.1 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF0067W PPA LNP* THERMOCOMP* UF0067W is a compound based on Polyphthalamide resin containing 30% glass fiber. Added features of this material include: Hot Water Moldable, Non-Brominated & Non-Chlorinated Flam.. |