Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 44.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific) LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 44.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural. |