Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC (Asia Pacific) LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific) LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 LNP* STAT-LOY* 9X03508 is a compound based on PPO+PA66 resin containing Proprietary Filler(s). Added features of this material include: Antistatic, Flame Retardant, High Impact. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 (Asia Pacific) LNP* Stat-loy* 9X03508 is a compound based on PPO+PA66 resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant, High Impact. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific) LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI (Asia Pacific) LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP (Asia Pacific) LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 LNP* THERMOCOMP* RF0029S is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific) LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AS PA 66 LNP THERMOCOMP* RF00AS is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT LNP* THERMOCOMP* WFB54 is a compound based on PBT resin containing 20% Glass Fiber, 25% Glass Bead. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP WFB54 PBT (Asia Pacific) LNP* Thermocomp* WFB54 is a compound based on Polybutylene Terephalate resin containing Glass Bead. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy .. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific) LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 43.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
24.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural. |