Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 36.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU LNP THERMOCOMP* GF006 is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 36.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP GF006XXZ PSU LNP THERMOCOMP* GF006XXZ is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 36.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon DX96690 PC LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America.. |