Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 29.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK
LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 29.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
16.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK
LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.