Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC (Asia Pacific) LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC (Asia Pacific) LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Asia Pacific) LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Europe-Africa-Middle East) LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer (Asia Pacific) LNP* Lubricomp* KCL34A is a compound based on Acetal Homopolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer (Asia Pacific) LNP* Lubricomp* KCL34A is a compound based on Acetal Homopolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific) LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific) LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |
|||
CTE, linear, Transverse to Flow | 27.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Europe-Africa-Middle East) Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e.. |