CTE, linear, Transverse to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QCL349 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, Flame Retardant, Elect..
CTE, linear, Transverse to Flow 19.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA6.10