Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 128 µm/m-°C @Temperature -40.0 - 40.0 °C |
71.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics REMEX VR4831 PBT 15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only |
|||
CTE, linear, Transverse to Flow | 128 µm/m-°C @Temperature -40.0 - 40.0 °C |
71.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics REMEX VR4831 PBT 15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only |
|||
CTE, linear, Transverse to Flow | 128 µm/m-°C @Temperature 25.6 - 93.3 °C |
71.0 µin/in-°F @Temperature 78.0 - 200 °F |
Diameter |
Saint-Gobain Rulon® 1410 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
CTE, linear, Transverse to Flow | 128 µm/m-°C @Temperature -40.0 - 40.0 °C |
71.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |
|||
CTE, linear, Transverse to Flow | 128 µm/m-°C @Temperature -40.0 - 40.0 °C |
71.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP LNP STAT-LOY* M3000 is a compound based on unfilled Polypropylene resin. Added feature of this material is: Antistat. |
|||
CTE, linear, Transverse to Flow | 128 µm/m-°C @Temperature -40.0 - 40.0 °C |
71.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP) LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s). |
|||
CTE, linear, Transverse to Flow | 128 µm/m-°C @Temperature -40.0 °C |
71.3 µin/in-°F @Temperature -40.0 °F |
ASTM D696 |
Dow SPECTRIM™ HH 390 Reaction Moldable Polymer Information provided by Dow |