Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 12.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.00 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by .. |
|||
CTE, linear, Transverse to Flow | 12.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.00 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI (Asia Pacific) LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by .. |
|||
CTE, linear, Transverse to Flow | 12.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.00 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 12.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.00 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific) LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 12.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.00 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 12.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.00 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific) LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber. |
|||
CTE, linear, Transverse to Flow | 12.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.00 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s). |