Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA (Asia Pacific) LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature -40.0 - 40.0 °C |
60.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature 23.0 - 55.0 °C |
60.0 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 108 µm/m-°C @Temperature 23.0 - 55.0 °C |
60.0 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers |