Polymer Property : CTE, linear, Parallel to Flow = 67.2 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature 23.0 - 55.0 °C
67.2 µin/in-°F

@Temperature 73.4 - 131 °F
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin
Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be..
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66
LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact, Wear Resistant.
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66
LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact, Wear Resistant.
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 (Asia Pacific)
LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact.
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 (Asia Pacific)
LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact.
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Asia Pacific)
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Asia Pacific)
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East)
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East)
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP)
LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s).
CTE, linear, Parallel to Flow 121 µm/m-°C

@Temperature -40.0 - 40.0 °C
67.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP)
LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s).