Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 17.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
9.83 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific) LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber. |
|||
CTE, linear, Parallel to Flow | 17.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
9.83 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive. |
|||
CTE, linear, Parallel to Flow | 17.7 µm/m-°C @Temperature -40.0 - 40.0 °C |
9.83 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific) LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |