Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 16.6 µm/m-°C

@Temperature -30.0 - 80.0 °C
9.22 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Europe-Africa-Middle East)