Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 160 µm/m-°C @Temperature 55.0 - 160 °C |
88.9 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
CTE, linear, Parallel to Flow | 160 µm/m-°C @Temperature 55.0 - 160 °C |
88.9 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
CTE, linear, Parallel to Flow | 160 µm/m-°C @Temperature 55.0 - 100 °C |
88.9 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro.. |
|||
CTE, linear, Parallel to Flow | 160 µm/m-°C @Temperature 55.0 - 160 °C |
88.9 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612
(Unverified Data**) Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided.. |