Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 160 - 249 °C |
7.78 µin/in-°F @Temperature 320 - 480 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatibilit.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 0.000 - 100 °C |
7.78 µin/in-°F @Temperature 32.0 - 212 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 150 - 250 °C |
7.78 µin/in-°F @Temperature 302 - 482 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 160 - 249 °C |
7.78 µin/in-°F @Temperature 320 - 480 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 160 - 250 °C |
7.78 µin/in-°F @Temperature 320 - 482 °F |
2 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 0.000 - 100 °C |
7.78 µin/in-°F @Temperature 32.0 - 212 °F |
2 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 150 - 250 °C |
7.78 µin/in-°F @Temperature 302 - 482 °F |
2 |
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, hig.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 160 - 250 °C |
7.78 µin/in-°F @Temperature 320 - 482 °F |
2 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 0.000 - 100 °C |
7.78 µin/in-°F @Temperature 32.0 - 212 °F |
2 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 150 - 250 °C |
7.78 µin/in-°F @Temperature 302 - 482 °F |
2 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications .. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 150 - 250 °C |
7.78 µin/in-°F @Temperature 302 - 482 °F |
2 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -40.0 - 150 °C |
7.78 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -40.0 - 150 °C |
7.78 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East) High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -40.0 - 150 °C |
7.78 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM SF2260 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 23.0 - 150 °C |
7.78 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM SF2350 PEI Blend High flow Ultem blends for thin wall application |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 23.0 - 150 °C |
7.78 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM SF2350 PEI Blend (Asia Pacific) High flow Ultem blends for thin wall application |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 23.0 - 150 °C |
7.78 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem SF2350 PEI Blend (Europe-Africa-Middle East) High flow Ultem blends for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.78 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DE004 PC LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.78 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific) LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.78 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DEL22P PC LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Electrically Conductive. Exceptional Processing, Wear.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 23.0 - 150 °C |
7.78 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
7.78 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DEL22P PC (Asia Pacific) LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature -40.0 - 150 °C |
7.78 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend High flow Ultem for thin wall application |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 0.000 - 100 °C |
7.78 µin/in-°F @Temperature 32.0 - 212 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 149 - 249 °C |
7.78 µin/in-°F @Temperature 300 - 480 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 149 - 249 °C |
7.78 µin/in-°F @Temperature 300 - 480 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
CTE, linear, Parallel to Flow | 14.0 µm/m-°C @Temperature 150 - 250 °C |
7.78 µin/in-°F @Temperature 302 - 482 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA)
(Unverified Data**) Amodel HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad.. |