Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing 25% Glass Fiber, 10% Graphite. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 357 PBT PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific) PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 357 PBT+PC PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 357U PBT Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific) Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL HN731A PPE+PS PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine.. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 357U PBT+PC Unreinforced PC/PBT, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific) Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific) Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |