Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® OQ3820 PC High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® OQ3820 PC (Asia Pacific) High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® OQ3820 PC (Europe-Africa-Middle East) High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific) LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® HX215HP PBT High Flow, Unreinforced, Polybutylene Terephthalate (PBT). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food conta.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® HX215HP PBT High Flow, Unreinforced, Polybutylene Terephthalate (PBT). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food conta.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® HX3061HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® HX3061HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 LNP* THERMOCOMP* RF0029S is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 (Asia Pacific) LNP* Thermocomp* RF0029S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to .. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
CTE, linear, Parallel to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East) A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |