Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Europe-Africa-Middle East) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® ML7652 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Medium flow, excellent low temperature ductility.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC (Asia Pacific) LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 LNP* FARADEX* PS003E is a compound based on Nylon 6 resin containing 15% Stainless Steel. Added features of this material include: EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Europe-Africa-Middle East) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing 10% PTFE and 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC (Asia Pacific) LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific) LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp KCL34 Acetal Copoly LNP* Lubricomp* KCL34 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
CTE, linear, Parallel to Flow | 70.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON ME003S PP LNP* STAT-KON* ME003S is a compound based on Polypropylene resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Heat Stabilized. |