Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific) LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific) LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature 60.0 - 138 °C |
34.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 855 PBT 15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature 60.0 - 138 °C |
34.0 µin/in-°F @Temperature 140 - 280 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 855 PBT (Asia Pacific) 15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -30.0 - 30.0 °C |
34.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East) DATA ON BK1005 ONLY. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -30.0 - 30.0 °C |
34.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+PS DATA ON BK1005 ONLY. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific) LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific) LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific) LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas re.. |