Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing 20% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific) LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 75-1/-2 |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 75-1/-2 |
BASF Ultrason® E 3010 MR UN PESU Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat.. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 75-1/-2 |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 75-1/-2 |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 52.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Asia Pacific) LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber. |