Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
ASTM E 831 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 55.0 - 160 °C |
278 µin/in-°F @Temperature 131 - 320 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 130 - 200 °C |
278 µin/in-°F @Temperature 266 - 392 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 23.0 - 55.0 °C |
278 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 23.0 - 55.0 °C |
278 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer
(Unverified Data**) Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 23.0 - 55.0 °C |
278 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100AL NC010 an unreinforced, high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication for low wear and friction against metals and plastics.Informat.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 55.0 - 100 °C |
278 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance.Information provided by DuPont Perf.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 527UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 527UV BK701 is a medium viscosity black acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvements in UV aging characteristics and ther.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 55.0 - 100 °C |
278 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers, pigmented red, having extremely low VOC emissions, developed for automotive interior applicatio.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 55.0 - 160 °C |
278 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 23.0 - 55.0 °C |
278 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSLR NC010 is a 25% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 55.0 - 160 °C |
278 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66
(Unverified Data**) Zytel® 80G14AHS BK099 is a 14% glass fiber reinforced, toughened, high flow, heat stabilized, black polyamide 66 resin. It offers outstanding performance in injection molding applications.Informati.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 55.0 - 160 °C |
278 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 23.0 - 55.0 °C |
278 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 55.0 - 160 °C |
278 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 55.0 - 100 °C |
278 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET
(Unverified Data**) Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 55.0 - 160 °C |
278 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 23.0 - 55.0 °C |
278 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 30.0 °C |
278 µin/in-°F @Temperature -40.0 - 86.0 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. It has been developed for consideration in applications and parts for th.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 55.0 - 160 °C |
278 µin/in-°F @Temperature 131 - 320 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® 545 BK504 PET
(Unverified Data**) Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature -40.0 - 23.0 °C |
278 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the.. |
|||
CTE, linear, Parallel to Flow | 500 µm/m-°C @Temperature 55.0 - 100 °C |
278 µin/in-°F @Temperature 131 - 212 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the.. |