Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL36S PA 66
LNP* LUBRICOMP* RFL36S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized.
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXY PA 66
LNP* LUBRICOMP* RFL36XXY is a compound based on Nylon 66 containing 30% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66
LNP* LUBRICOMP* RFL36XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 (Asia Pacific)
LNP Lubricomp is a compound based on PA66 resin containing glass fiber, PTFE. It is an internally lubricated compound that provide excellent chemical resistance, strength and wear/friction propertie..
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature 23.0 - 60.0 °C
21.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 (Asia Pacific)
LNP Lubricomp is a compound based on PA66 resin containing glass fiber, PTFE. It is an internally lubricated compound that provide excellent chemical resistance, strength and wear/friction propertie..
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC
LNP* THERMOCOMP* DX06409 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF004 PA 66
LNP THERMOCOMP* RF004 is a compound based on Nylon 66 resin containing 20% Glass Fiber.
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF004H PA 66
LNP* THERMOCOMP* RF004H is a compound based on Nylon 66 containing 20% Glass Fiber. Added feature of this grade is: Healthcare.
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66
LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber.
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific)
LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66
LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re..
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific)
LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66
LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Parallel to Flow 37.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DX06409 PC (Asia Pacific)
LNP* Thermocomp* DX06409 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.