Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 36.3 µm/m-°C @Temperature 40.0 - 120 °C |
20.2 µin/in-°F @Temperature 104 - 248 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive. |
|||
CTE, linear, Parallel to Flow | 36.3 µm/m-°C @Temperature 40.0 - 120 °C |
20.2 µin/in-°F @Temperature 104 - 248 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 compound |
|||
CTE, linear, Parallel to Flow | 36.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
20.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |