Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
11.7 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PPS Eco-FR compound |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature <=162 °C |
11.7 µin/in-°F @Temperature <=324 °F |
Below Tg; ISO 11359 |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 150 - 200 °C |
11.7 µin/in-°F @Temperature 302 - 392 °F |
4 |
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 150 - 200 °C |
11.7 µin/in-°F @Temperature 302 - 392 °F |
4 |
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount .. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 23.0 - 150 °C |
11.7 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Asia Pacific) PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump .. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -40.0 - 150 °C |
11.7 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 23.0 - 150 °C |
11.7 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -40.0 - 150 °C |
11.7 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 23.0 - 150 °C |
11.7 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature 23.0 - 150 °C |
11.7 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
CTE, linear, Parallel to Flow | 21.0 µm/m-°C @Temperature -40.0 - 150 °C |
11.7 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |