Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubriloy Z2000 PPE+PS LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP fo.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPE+PS (Asia Pacific) LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPO LNP* LUBRILOY* Z2000 is a compound based on PPO resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
45.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific) LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
45.6 µin/in-°F @Temperature 73.4 - 176 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH5110E PPE+PS (Europe-Africa-Middle East) NORYL NH5110E is a flame retardant, non halogenated, impact modified extrusion grade. Developed for low beard-growth, with a Vicat B/120 of 138 Deg C, according to ISO 306 and a UL-94 rating of V1@ .. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
45.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH5110E PPE+PS (Europe-Africa-Middle East) NORYL NH5110E is a flame retardant, non halogenated, impact modified extrusion grade. Developed for low beard-growth, with a Vicat B/120 of 138 Deg C, according to ISO 306 and a UL-94 rating of V1@ .. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Asia Pacific) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Asia Pacific) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Asia Pacific) Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Asia Pacific) Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |