Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific) PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Europe-Africa-Middle East) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re.. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Europe-Africa-Middle East) Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Asia Pacific) High flow PC+ABS material designed for local Pacific Automotive applications |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 4301 PPC+PC Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXRL0682 PC Copolymer 18 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® EXRL0683 PC Copolymer 11 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific) Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Europe-Africa-Middle East) Mold Release version of X7200This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific) High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer 40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer |
|||
CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |