Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 53.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Thermocomp PH0390A PA 6
LNP THERMOCOMP* PH0390A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 53.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp PH0390A PA 6
LNP THERMOCOMP* PH0390A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region.