Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 52.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 52.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 52.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 52.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 52.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 52.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 52.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing 20% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 52.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66 LNP* THERMOCOMP* RF00AH is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
CTE, linear, Parallel to Flow | 52.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66 (Asia Pacific) LNP* Thermocomp* RF00AH is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 52.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
29.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Asia Pacific) LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber. |