Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific) LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON ZE004 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON ZE004 PPO LNP* STAT-KON* ZE004 is a compound based on PPO resin containing 20% Carbon Fiber. Added feature of this grade includes: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK LNP* THERMOCOMP* LF003 is a compound based on Polyetheretherketone resin containing 15% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific) LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK (Asia Pacific) LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA6.10 LNP* LUBRICOMP* QCP36 is a compound based on Nylon 6/10 resin containing 15% PTFE/Silicone, 30% Carbon Fiber. Added features of this material include: Wear Resistant. Electrically Conductive |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66 LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RVL28 PA 66 LNP* VERTON* RVL28 is a compound based on Nylon 66 resin containing 40% Long Glass Fiber, 10% PTFE. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant, Structura.. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA 6/10 (Asia Pacific) LNP* Lubricomp* QCP36 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conducti.. |