Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific) LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI LNP THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing 30% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific) LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific) LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 (Asia Pacific) LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy .. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12 LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas .. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Verton NV006E PC/ABS LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas region.. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON NV006E PC/ABS (Asia Pacific) LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |
|||
CTE, linear, Parallel to Flow | 41.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
23.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON NV006E PC+ABS LNP* Verton* NV006E is a compound based on PC+ABS blend resin containing 30% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |